Abstract
To develop Pb-free piezoelectric ceramics, the dielectric and piezoelectric properties of NaNbO3–LiNbO3–SrTiO3 perovskite ceramics were investigated as functions of composition. As for ceramics prepared in this study, the orthorhombic perovskite phase was formed at lower temperatures and was transformed to a tetragonal form and then to a cubic form with an increase in temperature. The tetragonal-cubic transition temperature (Curie temperature, Tc) gradually shifted toward lower temperatures with an increase in SrTiO3 content. Among the ceramics obtained, the 0.86NaNbO3–0.09LiNbO3–0.05SrTiO3 composition showed relatively good piezoelectric properties, namely, kp = 0.20, d33 = 53 pC/N, and Qm = 500, for high-frequency applications for the Pb-free piezoelectric ceramics reproted.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.