Abstract

In this paper, we introduce a new Co precursor for the atomic layer deposition (ALD) of Co metal and other Co containing materials. CoCl2(TMEDA) (TMEDA = N,N,N′,N′-tetramethylethylenediamine) is a diamine adduct of cobalt(II) chloride that is inexpensive and easy to synthesize, making it an industrially viable precursor. Furthermore, CoCl2(TMEDA) shows good volatility at reasonably low temperatures and is thermally stable up to a temperature of ∼300 °C. We also present a full ALD study for the deposition of CoO thin films using CoCl2(TMEDA) and water as precursors. The process was investigated within a temperature range of 225–300 °C. Saturation of the film growth with respect to both precursor pulse lengths was verified. According to X-ray diffraction, the films were a mixture of hexagonal and cubic CoO. No reflections corresponding to Co3O4 were detected. The hexagonal phase is characteristic to nanomaterials only and is not seen in bulk CoO. The crystal structure of the films could be tuned by temperat...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call