Korea has developed an advanced reduced-activation alloy (ARAA) as a structural material for helium-cooled ceramic reflector test blanket module (HCCR-TBM) applications. The present paper describes the history of alloy development and the properties of ARAA, which has been produced at a 5t scale using vacuum induction melting and electro-slag re-melting methods. ARAA is a 9Cr–1.2W based ferritic–martensitic steel with 0.01wt.% Zr. The mechanical properties, thermal properties and physical and magnetic properties of ARAA show similar temperature dependencies to those observed for Eurofer 97. However, ARAA exhibits a much longer creep–rupture time than conventional RAFM steel, which suggests a positive effect on Zr addition. The enhanced creep strength of ARAA by the addition of Zr is attributed to the reduced temperature-dependence of the yield strength.