Abstract

In the present study, the effects of Ta content on the dynamic Young’s modulus and tensile properties of Ti−Ta alloys were investigated in order to find a Ti−Ta alloy that gives low modulus and high strength for biomedical applications. For this purpose, the ingots of Ti−Ta alloys with Ta contents from 10 to 50 mass % were melted, and then rolled into the plate of 3 mm thick. All the specimens were solution treated at 1223 K in the b field for 3.6 ks and then quenched in ice water. Subsequently, some of them were aged at 773 K for 259.2 ks followed by a rapid quenching in ice water. The corrosion capacity and biocompatibility of typical Ti−Ta alloy were also evaluated. The experimental results indicate that the Ti−30% Ta alloy has better mechanical biocompatibility, corrosion capacity and cyto-toxicity than Ti−6Al−4V alloy used as a standard biomaterial, and thus it will be of considerable development for biomedical applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.