Abstract

The development of texture and grain boundary character are researched for a boron bearing IF steel after recrystallization annealing for different times at 810°C. The results show that the main texture components are {111}<110> and {111}<112> after the cold rolling samples annealing different times. The maximal volume fraction of <111>//ND texture is about 78% for the sample annealing for 120sec. The main CSL boundaries are ∑3,∑5,∑7,∑9,∑11,∑13b and ∑17b. And the ∑3 grain boundary increase with increasing the annealing times from 60sec to 180sec.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.