Soy protein isolate film was reinforced with TiO2 nanoparticles. The effect of homogenization time and speed on mechanical and water barrier properties were tested by measuring thickness, swelling percentage, opacity, tensile strength (TS), elongation at break (Eb), water vapour permeability (WVP) and oxygen transmission rate (OTR). The thickness, opacity, TS and Eb of the film increased from 0.202 mm to 0.219 mm; 58.40% to 374.31%; 1.60 MPa to 3.20 MPa and 0.60% to 3.20% respectively and swelling percent, WVP and OTR decreased from 684.39% to 313.63%; 63.721 g/m2/day to 3.042 g/m2/day and 127.53cc/m2/day to 49.15 cc/m2/day respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.