Abstract

We developed the Ag-Mg-Sb alloy which had a tensile strength of about 500 MPa and elongation of 5.5%. The tensile strength of 150 MPa was obtained at room temperature in the Bi-2223 tape using this Ag-Mg alloy for the outer sheath. The J/sub c/ value of the Ag-Mg alloy sheathed Bi-2223 tape has come to be above 10/sup 4/ A/cm/sup 2/ at 77 K in self field. And the J/sub c/ value was kept until a tensile stress of 120 MPa was applied. The critical bending strain of the tape was the same as that of the pure Ag sheathed tape. These results indicated that this tape was tolerant of the mechanical stress in the manufacturing process and hoop stress during the magnet operation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.