Ni-based superalloys such as Alloy 706 that have high heat resistance are applied to gas turbine disks in electric power plant because. Free forging is one of the effective forging processes to form superalloy products, and forging simulation is quite useful method to optimize forging schedule. Softening behaviour at high temperature was not considered and implemented in conventional simulation, that induced the accuracy of load prediction. In this study, we investigated softening behaviour to improve the accuracy of forging simulation.