Abstract

AbstractOur multi-plume and multi-turn (MPT) pulsed-laser deposition (PLD) has been improved to accelerate reliable and fast deposition technique of high Ic (critical current) YBCO (YBa2Cu3O7-x) layer for a long coated conductor fabrication, for we increased the number of multi-turn, from three to four, in our multi-plume and multi-turn (MPT) PLD system. This increase of the number of depositing turns achieved high deposition rate corresponded to 75 mm3/h (=1 μm-thick × 10 mm-wide × 7.5 m/h, throughout all 4 turns) for YBCO layer. This four turn (4t)-MPT-PLD also indicated a capability to combine high deposition rate and high Ic. We attained the highest Ic's of 321 A at the tape speed of 3 m/h and 340 A at tape speed of 2 m/h by 4t-MPT-PLD in 10 mm-wide and 10 cm-long samples.Based on these results, we successfully deposited a 100 m long YBCO layer by 4t-MPT-PLD. This coated conductor had high Ic as high as 159 A, therefore, the multiplication of Ic and length exhibited high value of 15.9 kA·m.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.