The Fe3O4@C core/shell microspheres were fabricated via a two-step process. Fe3O4 microspheres were firstly prepared, and Fe3O4@C core/shell microspheres were subsequently fabricated using glucose as a carbon source by a hydrothermal route, in which the thickness of the carbon coating was about 20 nm. The resulting products were characterized by scanning electron microscope (SEM), transmission electron microscope (TEM), X-ray diffraction (XRD) and Fourier transform infrared spectra (FTIR). The Nitrogen adsorption–desorption isotherms reveal their mesoporous structure and larger BET surface area (62.3 m2g-1). The Fe3O4@C core/shell microspheres possess ferromagnetism and high saturation magnetization (39.2 emu ⋅ g-1). Bovine hemoglobin (BHb) was used as a model protein to test the adsorption and desorption properties of the Fe3O4@C core/shell microspheres. The capacity for BHb adsorption was more than 71.3 mg/g. According to the values obtained in the MTT (3-[4,5-dimethylthiazol-2-yl]-2,5-diphenyltetrazolium bromide) assay the Fe3O4@C core/shell microspheres show a low toxicity. Therefore, the prepared Fe3O4@C core/shell microspheres are of great significance for guided site-specific drug delivery.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.