Abstract

We studied relations between the microstructure and core loss of Mn-Zn ferrites for power supplies. As the results, we found that the lowest core loss was achieved at 100 kHz and 200 mT condition when the average grain size were 15 to 17 /spl mu/m. Then, we examined the effect of the third element in addition to CaO-SiO/sub 2/ on their deposition behavior in the grain boundary and we found the some additives such as Nb/sub 2/O/sub 5/, Ta/sub 2/O/sub 5/ and ZrO/sub 2/ which reduce the core loss. Further more, by optimizing the sintering condition, we were able to obtain the extremely low loss Mn-Zn ferrite material for power applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.