Abstract
Austenitic nickel-iron-chromium based superalloys are materials of choice for high temperature applications as they provide high temperature creep resistance associated with a suitable oxidation behavior in the temperature range of 600-1100°C. However, these properties are not sufficient for applications as Steam Methane Reformer (SMR). As a consequence, aluminum and chromium coatings are developed by the pack-cementation technique to improve their corrosion resistance. The oxidation behavior of the coated samples has been carried out in air at 1050°C. Chromium deposition leads to a layer of bcc chromium-iron solid solution. Oxidation tests indicated that a too high chromium concentration induces a too rapid growth of the chromia layer. In the case of aluminum coatings, a layer of -NiAl is formed at the surface of the alloy. It permits a significant decrease of the oxidation rate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.