Abstract Acid grade fluorite concentrate (AGFC) is the most valuable product of fluorite processing units. In this study, an environmentally friendly flowsheet is developed for the production of AGFC. The ore of the Kamar Mehdi fluorite mine (Tabas, Iran) is considered as a case study with grade of 76.65% fluorite, 21.62% dolomite and 0.32% hematite. The performance of ore flotation by changing operational parameters is evaluated in the presence of common and new fatty acid collectors, sodium oleate (SO) and sodium lauryl sarcosine (SLS), respectively. The best rougher concentrate (CaF2 = 88.49%) was obtained for 100 g/t of SLS and 500 g/t of dextrin at pH = 4. The concentrate is leached by acetic acid for the selective dissolution of dolomite. The acetic acid concentration of 0.31 M, the temperature of 80.33 °C, time of 126.29 min are chosen as optimum operational conditions using central composite design (CCD). It was found out the liquid to solid ratio of 4:1 is suitable for leaching purpose. AGFC containing 98.71% fluorite, 0.19% silica, and 0.05% sulfur is obtained by 91.55% dissolution of dolomite under these conditions. Finally, the calcium and magnesium acetate (CA & MA) is produced as an environmentally friendly by-product through the crystallization of the leaching filtrate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.