Tl-1223 tapes with engineering critical current densities, (E-J/sub c/) values of 2500 Acm/sup -2/ can be routinely fabricated but the magnetic field properties are poor due to weak link effects. We have developed a partial melt processing route which results in increased grain growth with greater potential for achieving grain alignment. We have investigated the effect of Tl-1223 phase composition on the melt process and found that Bi substitutions lead to an increased grain size in tapes made using unreacted powder but a decrease in grain growth in tapes made with reacted powder.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.