Abstract

The development and evolution of texture in a Mg–10.6%wt Zr deposit obtained by physical vapor deposition was studied. The deposit exhibits a microstructure characterized by elongated grains with the [0001] direction parallel to the deposit growth direction. The volume fraction of the basal plane component increases throughout the thickness from 45% at the collector side up to around 70%. The minimization of interfacial energy of (0001) planes induces the initial texture at the earliest stage of the deposit formation. Furthermore, the increase in the volume fraction of the (0001) component during deposit growth is provoked by texture competition, which results in the development of grains with the [0001] direction parallel to the deposit growth direction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.