Abstract

Abstract This paper deals with the issues pertinent to the design of frost-resistant concretes in exposure class XF3 (high water saturation) when the concretes are made with cements containing ground granulated blast furnace slag (ggbs). The testing programme covered four series of non-air entrained concrete made with cements CEM I, CEM II/A-S, CEM II/B-S and CEM III/A containing 0%, 13%, 28% and 53% ggbs respectively, and two non-air entrained concrete series with the binder made from CEM I and 0 to 55% ggbs. The water-binder (w/b) ratio ranged from 0.25 to 0.55. Frost durability testing was performed using a modified ASTM C666A procedure to determine changes in mass (dm) and beam length (dL). The relationships occurring between the w/b ratio and ggbs content in the binder and the length change (dL) of the specimens were described using curvilinear regression functions, through the analysis of artificial neural networks. Slag-content-dependent critical values of the w/b ratio were determined taking the length change dL = 1.3 mm to be the criterion for the resistance to internal cracking. In the authors’ view, this approach can be a good method for checking equivalent performance of concretes made with cements containing mineral additions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.