The behaviour of iron in the Bayer process has been investigated by neutron activation analysis and Ge(Li) spectrometry, using bauxite samples of various origin. The amount of iron impurities in alumina was found to be independent of the origin of the bauxites. Alumina is contaminated by iron in the process of decomposition of aluminate liquors; regardless whether iron is present in ‘dissolved’ form or as a floating impurity, it will pass into the alumina almost completely.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.