Abstract
A new method for determining the fibre saturation point (FSP) of whole never-dried wood is described. Enthalpy of melting values from differential scanning calorimetry (DSC) experiments are used to calculate the proportion of non-freezing water. Two methods for calculating the FSP from the enthalpy data are described. FSP determinations were carried out on the commercially important West Australian eucalypt species, Eucalyptus marginata and Eucalyptus diversicolor and a plantation softwood, Pinus radiata. Results are reproducible and are corroborated by the traditional volumetric shrinkage method for determining the FSP. On all samples below 10 mg a low temperature endothermic peak is observed as a shoulder on the main peak. It is postulated that this is due to an intermediate layer of water between the freezing and non-freezing water.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.