The diffusion coefficient of water into thin polymer layers of glutar aldehyde cross-linked atelocollagen type I matrix (sample 1, the typical layer thickness was about 0.065 × 10−3 m) at 23 °C was 1.142 × 10−10 m2 s−1. At twice the concentration of the cross-linking agent (sample 2) the diffusion coefficient was 2.795 × 10−10 m2 s−1. This increase was attributed to the more ordered morphology and the creation of ordered microvoids in the film. A larger surface area is then available for the transport of diffusing molecules, allowing a higher penetration rate of the solvent.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.