Abstract

A sensitive method was used to measure the content of styrene-butadiene rubber(SBR) in modified asphalt by HPLC.The temperature was set at 30 ℃ and a wavelength of 222 nm was used for the detector.A mobile phase of hexane,acetonitrile and THF with equal proportion was used.The RSD of this method is 1.5%,and a linear equation of y=800.94x+579.03 with a correlation coefficient of r=0.9998 was obtained.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.