Abstract

Investigations of the defect structure of a gradient-activated stoichiometric LiNbO3:Mg2+, Cr3+ crystal, in which the chromium concentration has a constant value of 0.1 at. % along the crystal growth axis, and the magnesium concentration changes smoothly from 5.5 to 2.0 al. %. The threshold concentration of Mg2+ ions (2.35 at. %) in these crystals with a concentration width of change in the center composition (Cr optical center and its nearest neighbors) of 0.09 at. % Mg2+ ions is established..

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.