The authors measured the adiabatic dielectric permittivity epsilon b of tris-sarcosine calcium chloride (TSCC) at 400 Hz near the ferroelectric transition for DC bias fields up to 5000 V cm-1. They found epsilon infinity =4.2+or-0.2, Curie-Weiss constant C+=38.3+or-0.3K, T0=129.4+or-0.1K, and Landau coefficients A=(2.95+or-0.2)*109 V m A-1 s-1 K-1 and B=(3.5+or-0.1)*1015 V m5 A-3 s-3. They observed evidence of an internal bias field as reported previously by others.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.