Abstract
Abstract Fracture toughness of a material that undergoes pop-in crack extension was measured in two different heat treated conditions by a new procedure proposed in a recent publication. It is shown in this publication that the new procedure gives a size independent plane strain fracture toughness KIc value in thin and wide specimens prepared from relatively tough material. The present investigation examines the effect of width and the applicability of various approaches to fracture toughness measurement procedures, such as the new procedure, ASTM Test Method for Plane-Strain Fracture Toughness of Metallic Material (E 399), KIc, the ductile fracture toughness value JIc, and the crack growth resistance R curve, to a material that undergoes pop-in crack extension. The results show that whereas the new procedure can give a meaningful, reliable, and size independent fracture toughness even for a material that undergoes pop-in crack extension, the other methods, such as R curve, JIc, Kpop, or ASTM E 399 are inapplicable. The new procedure also shows that the K-KIc approach can be used in specimens whose thickness is 4.5 times less than that required by ASTM E 399.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.