Abstract
Abstract Waste paper, the use of which is increasing day by day as a raw material, has a heterogeneous structure as it contains non-fiber material from different sources. It is desired to have a homogeneous product when recycled. Within the scope of this study, the SEM images of the raw materials determined according to EN 643 standard and the products made with the recycling of these raw materials were examined, ash content, fines content and ash on sieve were stated and the results obtained by determining filler content (removed) and fiber fines (removed) were discussed. While the samples with the highest ash content were H3 and U3, the lowest samples were H6 and U9. It was determined that the samples with the highest fines content were H2 and U1, while the lowest samples were H4 and U2. While the samples with the highest ash on sieve were H3 and U3, the samples with the least were determined as H2 and U9. The filler content was highest in H1 and U3 samples, while the lowest was in H6 and U9 samples. The samples with the most fiber fines were found as H2 and U9, and the least as H1 and U3 samples.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.