High pressure crystallized linear polyethylene was treated with fuming nitric acid and of both samples treated and untreated the X-ray wide angle line widths of 18 hkl-reflections were analysed. The three axes and the orientation of the mean shape ellipsoid and thegki-values of the paracrystalline distortions were determined. The crystallite size perpendicular to the chain direction is up to 1650 A and parallel to the chain direction higher than 5000 A and is not be changed significantly by HNO3-treatment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.