Extruded polystyrene (XPS) is often treated with hexabromocyclododecane (HBCD) as fire retardant (FR). Because of its aliphatic structure, HBCD is not suspected to cause formation of polybrominated dioxins upon combustion. Precursors of polybrominated dioxins, namely bromophenols, were detected during tubular furnace combustion experiments of FR-XPS in combination with sorptive enrichment on polydimethylsiloxane followed by on-line thermal desorption-capillary GC/MS. The highest concentration of mono- and tribromophenols detected were 85.9 and 3.7 mg kg −1, respectively, at a temperature of 700 °C, while a temperature of 500 °C yielded the highest concentration of dibromophenols namely 10.4 mg kg −1. At a combustion temperature of 900 °C no bromophenols were detected.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.