The new technique has been developed for measuring the β-transus temperature of (α+β)-titanium alloys with any initial microstructure by means of the DSC method. The technique is based on a linear correlation between extremums of temperature on the DSC time-derivative curve, the Mo-equivalent of an alloy and the equilibrium β-transus temperature. The developed technique enables the determination of the β-transus temperature with the use of a single specimen and it is characterized by high accuracy comparable with that of structural analysis techniques.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.