Abstract

We present an X-ray absorption spectroscopy study on Fe-doped SrTiO3 thin films grown by pulsed laser deposition. The Fe L2,3 edge spectra are recorded for doping concentrations from 0-5% after several annealing steps at moderate temperatures. The Fe valence state is determined by comparison with an ilmenite reference sample and calculations according to the charge transfer multiplet model. We found clear evidence of Fe(2+) and Fe(3+) oxidation states independently of the doping concentration. The Fe(2+) signal is enhanced at the surface and increases after annealing. The Fe(2+) configuration is in contrast to the mixed Fe(3+)/Fe(4+) valence state in bulk material and must be explained by the specific defect structure of the thin films due to the kinetically limited growth which induces a high concentration of oxygen vacancies.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.