Abstract

Recording resolution, medium noise and thermal stability have been investigated for double layered perpendicular magnetic recording media. The recording performance was improved by introducing a stacked intermediate layer between a soft magnetic backlayer and a storage layer due to increased crystal orientation with a small magnetic domain size and suppressed initial growing layer of the storage layer. The reproduced output at an extremely high linear density of 950 kFRPI was detected by using a contact-type CF-SPT head for write and a GMR head with a narrow read track width of 0.4 μm.