Abstract
The use of large volume sealed stainless steel capsules has allowed the measurement of a transition temperature in wool at a range of moisture contents using differential scanning calorimetry. Aged wool showed an endothermic peak that disappeared after cooling from above the transition temperature, but was restored with subsequent ageing at ambient temperature. Similar behavior is characteristic of amorphous polymers annealed below their glass transition temperature. Moisture appeared to act as a plasticizer in wool and lowered the transition temperature. At moisture contents of 22% the transition temperature approached 35°C, and the application of this result to the formation of severe wrinkles in wool garments during wear is discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.