Abstract
Silver-zinc-nickel spinel ferrite was prepared by the co-precipitation procedure with the precise composition Ag0.1Zn0.4Ni0.5Fe2O4 for bolstering pollutant removal effectiveness while upholding magnetic properties and then coated with a mesoporous silica layer. The surface characteristics and composition of Ag0.1Zn0.4Ni0.5Fe2O4@mSiO2 were confirmed using EDX, FT-IR, VSM, XRD, TEM, SEM, and BET methods. The surface modification of Ag-Zn-Ni ferrite with a silica layer improves the texture properties, where the specific surface area and average pore size of the spinel ferrite rose to 180 m2/g and 3.15 nm, respectively. The prepared spinel ferrite@mSiO2 has been utilized as an efficient adsorbent for eliminating methyl green (MG) and indigo carmine (IC) as models of cationic and anionic dyes from wastewater, respectively. Studying pH, Pzc, adsorbent dosage, dye concentration, and temperature showed that efficient removal of MG was carried out in alkaline media (pH = 12), while the acid medium (pH = 2) was effective for IC removal. Langmuir isotherm and pseudo-second-order kinetics were found to be good fits for the adsorption data. Both dyes were adsorbed in a spontaneous, endothermic process. A possible mechanism for dye removal has been proposed. The adsorbent was effectively recovered and reused.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.