In a recent study, 25 development-length tests were conducted on rectangular and T-shaped semilightweight beams having design compressive strengths of 48 MPa (7,000 psi) and 69 MPa (10,000 psi). In the rectangular beam tests, the design moment capacity was exceeded in every case. However, in the tests on T-shaped beams, bond failure occurred in some specimens immediately after the formation of a flexure-shear crack. Additional tests were then conducted on similar T-shaped beams having varying amounts of transverse reinforcement near the point load. These tests showed that bond failure could be prevented by increasing the transverse reinforcement near the point of maximum moment. The study showed that the shift in the tension force that occurs when flexural cracks turn diagonally may lead to bond failure if sufficient anchorage of the strand is not provided. Therefore, the investigators recommend that the current AASHTO requirements for strand development be enforced at a “critical section” located at a distance dp from the point of maximum moment toward the free end of the strand, where dp is the distance from the extreme compression fiber to the centroid of the prestressed reinforcement.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.