Abstract
AbstractSummary: A method of depth profiling by AFM nanoindentations is developed for the characterisation of the heterogeneity of the mechanical properties of oxidised polymers. An increase or a decrease of the sample stiffness is measured close to the surface. A comparison with micro‐FTIR profiles and a knowledge of the photooxidation mechanism permit an interpretation of the chemical and physical changes and give new insights into the understanding of the ageing behaviour.Photooxidation profile of a TMPC film measured by AFM (•) and by micro‐FTIR (♦) after irradiation.imagePhotooxidation profile of a TMPC film measured by AFM (•) and by micro‐FTIR (♦) after irradiation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.