Abstract Specimens of polycrystalline UO2 were strained in compression at constant strain rate from 0.05 to 10.0/min and at temperatures ranging 900°–2,000°C. The experimental results revealed characteristic yield point, and the yield stress varied with strain rate and temperature. The present data, obtained at strain rates higher than currently adopted, showed greater sensitivity on strain rate and a higher activation energy for yield flow. The data are discussed in their relation to the mechanism that controls the yield strength. The yield strength at high strain rate would appear to be controlled primarily by the peierls stress.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.