Abstract
Morphology, crystallinity and electrochemical properties of Si powders fabricated by a mechanical milling process with milling time of 6-40 h were investigated by means of FESEM, XRD, Raman, TEM and cell test. Average size of Si powders was reduced to sub-micrometer scale after 10 h-milling and 40 nm-Si powders could be obtained at 48 h-milling. With increasing milling time, Si powders mostly changes from crystalline Si to amorphous one and the content of amorphous Si was increased. TEM result showed that a negligiable amount of crystalline Si remained even after 48 h-milling. Si electrode with 48 h-milled Si powders exhibited the best electrochemical properties in terms of capacity, efficiency and cycle performance: initial capacity of 3025 mAh g(-1), coulrombic efficiency of 79.4% and the capacity retention of 1000 mAh g(-1) (at 130 cycles). The good electrochemical properties of nano- and amorphous-Si are due to the high resistance against volume change and good reversibility of Li ion.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.