Abstract In this study, the hydrogen absorption and desorption condition was investigated after partial substitution of commercial V–Fe alloy for Cr in TiCr 1.8 alloy and the hydrogen storage capacity of TiCr 1.8− X (VFe) X ( X =0, 0.2, 0.4, and 0.6) was examined. Results of pressure–composition isotherm (PCI) tests showed that the maximum hydrogen storage capacity increased with increasing V–Fe content. TiCr 1.2 (VFe) 0.6 had the highest maximum and reversible hydrogen storage capacity in the range of low temperature. X-ray diffraction (XRD) patterns of the alloys became simpler with the increase of V–Fe content. The crystal cell parameters increased simultaneously.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.