Abstract

Abstract In this paper, yarns of photocatalyst modified polyester staple fiber, cotton and blended yarn of bamboo fiber and photocatalyst modified polyester were selected. Series of woven fabric were manufactured.The photocatalyst fiber contents of woven fabrics were changed from 0% to 100% with 20% gap, that is 0%,40%,60%,80% and 100%. The deodorant performance of these fabrics were tested and analyzed, it can be concluded that when the content of the photocatalyst is 80% or 100%, the fabrics owns better deodorant; when the photocatalyst content in fabric is 40% or 60%, it has the deodorantion properties but the effect was not good. It can be shown from this experimental study that the deodorizing fabrics can be considered to develop if only the content of photocatalyst is above the 80%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.