Abstract

This paper discusses the dependence of the mechanical properties and microstructure of sintered hydroxyapatite (HA) on the sintering temperature and pressure. A set of specimens was prepared from as-received HA powder and sintered by using a spark plasma sintering (SPS) process. The sintering pressures were set at 22.3MPa, 44.6MPa, and 66.9MPa, and sintering was performed in the temperature range from 800°Cto1000°C at each pressure. Mechanisms underlying the interrelated temperature-mechanical and pressure-mechanical properties of dense HA were investigated. The effects of temperature and pressure on the flexural strength, Young’s modulus, fracture toughness, relative density, activation energy, phase stability, and microstructure were assessed. The relative density and grain size increased with an increase in the temperature. The flexural strength and Young’s modulus increased with an increase in the temperature, giving maximum values of 131.5MPa and 75.6GPa, respectively, at a critical temperature of 950°C and 44.6MPa, and the fracture toughness was 1.4MPam1∕2 at 1000°C at 44.6MPa. Increasing the sintering pressure led to acceleration of the densification of HA.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call