Abstract

A systematic study on the densification behavior and build quality of 2205 duplex stainless steel fabricated using laser powder bed fusion (LPBF) was performed by experiment and simulation, aiming to offer some supplementary work for research on additive manufacturing (AM) of duplex stainless steel. In this study, samples with differing laser powers were prepared, and a highest relative density of 98.87% was obtained. Then, the pore defects and surface morphologies were investigated to unveil densification behaviors during a building process. The relationship between surface morphologies and the formation of pores was discussed. It reveals that the inter-layer printing on these surface defects caused by unreasonable laser power could increase the possibility of inside pore defects and reduce the density of specimens. Particularly, the big spatters could be the cause of lack-of-fusion defects even under sufficient power input. Therefore, adequate intra- and inter-layer bonding under reasonable processing parameters is crucial for densification. The mechanical properties of the specimens prepared with the laser power of 260 W are the highest, and the yield strength, tensile strength, and elongation are 798.68 MPa, 953.63 MPa, and 10.85%, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.