Abstract

Potassium tantalate (KTaO3) is a promising material for dielectric applications at low temperature. However, dense and single-phase ceramics cannot be obtained by conventional sintering because of the evaporation of potassium that leads to secondary phases. Here, we demonstrate that spark plasma sintering is a suitable method to obtain dense and single-phase KTaO3 ceramics, by optimizing three parameters: initial composition, temperature, and pressure. A 2 mol% K-excess in the precursors leads to a large grain growth and dense single-phase ceramics. Without K-excess, a small amount of secondary phase (K6Ta10.8O30) is observed at the surface but can be removed by polishing. At ∼10 K, the dielectric permittivity is 4 times higher in the ceramic from the 2 mol% K-excess powder, because of the larger grain size. The thermal conductivity decreases with decreasing grain size and stays above the thermal conductivity of KNbO3 ceramics.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call