Abstract

Dealloyed ribbons with a layer of networked nanoporous structure of different pore sizes were fabricated by dealloying the as-spun Mg65Cu25−xAgxY10 (x=0, 5, 10, at.%) ribbons in dilute H2SO4 solution in order to enhance the degradation efficiency of pesticide wastewater. Compared to the as-spun ribbons, it is found that the dealloyed ribbons with the networked nanoporous structure exhibit higher degradation efficiency due to their large specific surface areas and enough active sites for the degradation process. Both the average pore sizes of the nanoporous structure and the degradation efficiency of the pesticide wastewater increase with the increase of Ag addition in the dealloyed ribbons. The maximum degradation efficiency up to 95.8% is obtained for the Mg65Cu15Ag10Y10 dealloyed ribbon under the optimal conditions of pH being 3, the initial cis-cypermethrin concentration being 500 mg/L, and the dosage of dealloyed ribbon being 1.33 g/L.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.