Abstract
Cross sections through nanoindents on Si, Ge, and GaAs {001} were examined through transmission electron microscopy. A focused ion beam workstation was used to machine electron transparent windows through the indents. In both Si and Ge there was a transformed zone immediately under the indent composed of amorphous material and a mixture of face-centered-cubic and body-centered cubic crystals. Cracking and dislocation generation were also observed around the transformed zone. In GaAs the dominant deformation mechanism was twinning on the {11} planes. The hardness of these materials is discussed in light of these observations and their macroscopic material properties such as phase transformation pressure.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.