Abstract

Proton irradiation tests have been performed on two cold-worked zirconium specimens using 4.4 MeV protons with controlled displacement damage rates between 1.4 and 6.9 × 10 −7 dpa s −1. The specimens had different Fe contents, nominally pure (NP): 64–70 ppm by weight, and ultra-high purity (UP): 3–5 ppm by weight. A stress of 50 MPa was applied during the tests, and the test temperature was 347 K.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.