We observed an unexpected bending of a horizontally held palladium plate at 150°C under a small external shearing stress. The deformation was fastest at the nominal composition of PdH0.1−0.2, which is in the α+β phase. We also observed that a plate warped back and forth during a cycle of absorption and desorption of hydrogen when it was hung vertically, which does not have a reasonable explanation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.