Abstract

Instead of applying severe plastic deformation, high-temperature heat treatment or high pressure, grain refinement and high-temperature phase separation induced by deformation in single-phase body-centered-cubic (bcc) coarse-grained Co–Fe alloys have been achieved by simple room-temperature compression. The alloys exhibit large plasticity over 140% without fracture. Phase separation from the bcc phase to nanoscale face-centered-cubic Fe and Co phases, which generally occurs at high temperature above ∼1150K, is formed in the deformed samples. The possible mechanisms are shear deformation and deformation-enhanced atomic diffusion rather than the temperature rise during deformation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.