Abstract

A defects evolution below the surface in nickel aluminum bronzeCuAl9Ni4Fe4 subjected to cavitation under mild conditions with times up to 8 hwas studied using positron annihilation spectroscopy, mass loss measurements, and scanning electron and atomic force microscopies. The obtained results indicate two different stages of cavitation erosion. At the beginning of cavitation up to 6 h in incubation period a removing of residual roughness and surface oxides was noted. Then, in the maximal erosion rate region, big vacancy clusters were recognized and their concentration drastically increases around 100 times in comparison with the incubation period.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.