Abstract

In this paper, 6013-T4 T-joints were successfully fabricated with different welding parameters by friction stir welding in two different combination modes of skins and stringers. The distribution features and formation mechanisms of defects in T-joints were observed and analyzed. The effect of defects and welding parameters on tensile properties of T-joints was investigated. The result shows that the T-joint without tunnel defect only can be obtained with the traverse speed of 100mm/min in this experiment, and the welding parameters influence the features and sizes of kissing bond defects. The fracture of T-joints along the shin is attributed to the kissing bond defect and the tunnel defect is the main factor affecting the tensile properties along the stringer.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.