Abstract

AbstractA polycrystalline silicon (pc-Si) thin film with large grains on a low-cost non-Si substrate is a promising material for thin-film solar cells. One possibility to grow such a pc-Si layer is by aluminum-induced crystallization (AIC) followed by epitaxial thickening. The best cell efficiency we have achieved so far with such an AIC approach is 8%. The main factor that limits the efficiency of our pc-Si solar cells at present is the presence of many intra-grain defects. These intra-grain defects originate within the AIC seed layer. The defect density of the layers can be determined by chemical defect etching. This technique is well suited for our epitaxial layers but relatively hard to execute directly on the seed layers. This paper presents a way to reveal the defects present in thin and highly-aluminum-doped AIC seed layers by using defect etching. We used diluted Schimmel and diluted Wright etching solutions. SEM pictures show the presence of intra-grain defects and grain boundaries in seed layers after defect etching, as verified by EBSD analyses. The SEM images of diluted Wright etched pc-Si seed layer shows that grain boundaries become much better visible than with diluted Schimmel etch.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.