Abstract

BaBi4Ti4−x(Cu0.5W0.5)xO15 ceramics with Cu2+ and W6+ co-substitution for the B-site Ti4+ were prepared by using the solid-state reaction process. It was desirable that piezoelectric properties of the BaBi4Ti4−x(Cu0.5W0.5)xO15 ceramics could be improved by inducing the larger lattice distortion with the oxygen vacancy defects neutralized and restrained. Results of the X-ray diffraction analysis confirmed that crystal cell parameter c decreased obviously with the increase in the crystal cell parameter a. Curie temperature, resistivity, and piezoelectric properties of the BBT ceramics are improved by the copper and tungsten modification. The maximum value of piezoelectric coefficient (~ 30 pC/N) can be obtained in the BaBi4Ti4−x(Cu0.5W0.5)xO15 ceramics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.