Abstract

This paper reports on a hydrogen storage material of poly(methyl acrylate) and methylamine borane (PMA/MeAB) composite, which is synthesized by a simple solution-blending process at room temperature. The thermal decomposition process of the as-prepared composite is investigated by temperature programmed desorption/mass spectrometer (TPD/MS), thermogravimetry (TG) measurements and water displacement method. It is found that PMA/MeAB100 (100 mg PMA with 100 mg MeAB) starts to release H2 at the temperature of 90.5 °C with the dehydrogenation peak centered at 120.7 °C. This is about 20 °C lower than that of neat MeAB. Meanwhile, the evaporation of MeAB and the volatile byproducts from the dehydrogenation stage of PMA/MeAB100 are also suppressed. The present result shows that the dehydrogenation property of MeAB is enhanced by using PMA/MeAB composite.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.